Properties:
- Low free alkali content
- Good flank adhesion
- Low inherent stress
- UV-resistant pigments
- Can be made hydrophobic
Storage / shelf life:
If stored in an unopened container and in a dry place, the product will keep for approx. 12 months.
Application rate:
- Approx. 1.6 kg/l cavity volume
- Apply to a large enough trial area to determine the precise amount required
Application instructions:
Once it has hardened, mortar must not be made workable again by adding either water or more wet mortar.
The type and duration of the reworking and surface treatment will influence the colour.
Slight deviations in colour between different batches are possible.
Protect wet mortar surfaces against frost, rain and drying out too quickly for at least 4 days.
Tips on use:
Once it has hardened, mortar must not be made workable again by adding either water or more wet mortar.
The type and duration of the reworking and surface treatment will influence the colour.
Slight deviations in colour between different batches are possible.
Protect wet mortar surfaces against frost, rain and drying out too quickly for at least 4 days.Properties:
- Low free alkali content
- Good flank adhesion
- Low inherent stress
- UV-resistant pigments
- Can be made hydrophobic
Storage / shelf life:
If stored in an unopened container and in a dry place, the product will keep for approx. 12 months.
Application rate:
- Approx. 1.6 kg/l cavity volume
- Apply to a large enough trial area to determine the precise amount required
Application instructions:
Once it has hardened, mortar must not be made workable again by adding either water or more wet mortar.
The type and duration of the reworking and surface treatment will influence the colour.
Slight deviations in colour between different batches are possible.
Protect wet mortar surfaces against frost, rain and drying out too quickly for at least 4 days.
Tips on use:
Once it has hardened, mortar must not be made workable again by adding either water or more wet mortar.
The type and duration of the reworking and surface treatment will influence the colour.
Slight deviations in colour between different batches are possible.
Protect wet mortar surfaces against frost, rain and drying out too quickly for at least 4 days.